Inombolo yomkhiqizo | Igama Lomkhiqizo | Ukubukeka | Ingxenye Eqinile Ngaphezulu kwamahora angu-120 3 | I-Viscosity (Tu-1 inkomishi 25°C) | Ukunamathela (Penta imitha yefilimu) | Yomile (Ukuthinta ngomunwe) | Cukuhlukumeza | Ingxenye eyinhloko |
JY-3200 | I-PU seal primer | Uketshezi olumhlophe olukhanyayo | 60±5% | 20+2KU | ≥95% | ≥20 min | Kulula ukwenza isihlabathi, ubulukhuni obuhle | Ama-resin e-polyurethane agcwele |
I-JY-3210 | I-PU yesibili degree primer | Uketshezi olumhlophe olukhanyayo | 60±5% | 50+2KU | ≥95% | ≥20 min | Kulula ukwenza isihlabathi, ubulukhuni obuhle | |
I-JY-3220 | I-PU yesibili degree primer | Uketshezi olumhlophe olukhanyayo | 60±5% | 55+2KU | ≥95% | ≥20 min | Kulula ukwenza isihlabathi, ubulukhuni obuhle |
1: I-ejenti eyinhloko kufanele isetshenziswe ne-hardener ehambisanayo, isilinganiso singu-2: 1, i-viscosity yokwakha inconywa ukuba ibe imizuzwana engu-15 ~ 18, umsebenzisi angashintshwa ngokuvumelana nesimo esithile.
2: Indawo yokwakha kufanele ibe ngaphezu kuka-15℃ ukuze kuqinisekiswe ukusebenza kabusha kwe-ejenti eyinhloko ne-hardener.
3: Ukuze kusetshenziswe ifilimu ngemva kokumisa sanding kungenziwa kabusha camera noma umunwe touch akusho ibala izandla ngaphandle sanding kungenziwa kabusha camera izikhathi eziningana zilandelana.Ukusandeni ngemva kokumiswa.
Ukusandwa kwesitoko (Quercus, Ash)Isigcwalisi (impahla enezimbotshana ezinkulu) Eyomile nesihlabathi,I-PU headiness (iphayini, i-teak nezinye izinkuni ezinamafutha)>240 # i-sandpaper
I-PU 2nd degree primer (kuze kugcwaliswe) okomile kwe-sanding PU topcoat (noma i-PE, NC topcoat) ukugoqa okomile;
1: Ibhodi kufanele ligweme ukungcoliswa kwamanzi futhi okuqukethwe kwamanzi akufanele kube ngaphezu kuka-12%.
2: Ngemuva kokuxuba i-ejenti eyinhloko kanye ne-hardener, qhubeka nokusebenzisa ngesikhathi esitholakalayo, imishini yokufafaza ukugeza ngesikhathi esifanele.
I-3: Lolu lwazi lusethwe ngaphansi kwesimo senkampani yethu, ukuze lusetshenziswe kuphela.